Releasing too Tight
Published:2021-07-07 18:23:32    Text Size:【BIG】【MEDIUM】【SMALL

Problem: The printing pattern is too big, and the glue viscosity, glue solvent penetration are very strong, it will cause dissolution between the printing glue and the releasing layer. As a result, the cut edge releasing become very tight, the color also changes, there will be wrinkling and bad small ...etc problem.

Solution: Pay attention to adjusting the ratio of solvents (primary solvent, secondary solvent, auxiliary solvent), and try to reduce the ratio of strong solvents. At the same time, adjust the viscosity of the glue, increase the solid content, and reduce the penetration strength.